Typical characteristics | Method | МГЕ-46В |
---|---|---|
Kinematic Viscosity - at 100 °С, mm²/s - at 50 °С, mm²/s |
ГОСТ 33 ГОСТ 33 |
6.7 46.4 |
Flash Point (COC), °С | ГОСТ 4333 | 227 |
Pour Point, °С | ГОСТ 20287 | - 33 |
Total Acid Number, mg KOH/g | ГОСТ 11362 | 0.95 |
Density - at 15 °С, kg/m³ |
ASTM D 4052 |
881 |
Viscosity Index | ГОСТ 25371 | 95 |
Tribological characteristics, Four-Ball Method - Wear Scar Diameter, mm |
ГОСТ 9490 |
0.31 |